I was thinking you could also split the halves again on the lateral line that runs from the gill cover to tail so the air hammer could get up inside to shape after the welding (or at least tacking) is done. You could really do some fine tuning that way.

Last edited by mark g; 01-25-2021 at 09:57 PM.