Default

I worked with a Porsche (935) race team in 1982 and their weld guy used that method for sharpening tungs.
Seems okay and the chem does not seem to affect Fe, AL, SiBr and etc. don't know the limits, but maybe Ti would reflect the chem in the welds?

He used it because it was a "clean" shop with no abrasives used at all.
__________________
Kent

http://www.tinmantech.com

"All it takes is a little practical experience to blow the he!! out of a perfectly good theory." --- Lloyd Rosenquist, charter member AWS, 1919.
Reply With Quote
 

Thread Tools Search this Thread
Search this Thread:

Advanced Search
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is On
HTML code is Off

Forum Jump

All times are GMT -5. The time now is 05:15 AM.

Powered by vBulletin® Version 3.8.11
Copyright ©2000 - 2024, vBulletin Solutions Inc.