Quote:
Originally Posted by robtg View Post
I called Tm Technologies with that same question and was told to use it, no problem. I have been using it for a few months now without any problems. I just break off a chunk and mix with water. ---RG
Right-o.
If the flux is clean and free of fly offal and bug spewtle then it is ready to use. So grab a clean stub of wood dowel and do the polka with the end of it in the jar to break up the chunks back into powder, measure out, and mix with H20 and go.
__________________
Kent

http://www.tinmantech.com

"All it takes is a little practical experience to blow the he!! out of a perfectly good theory." --- Lloyd Rosenquist, charter member AWS, 1919.