Quote:
Originally Posted by zekeymonkey View Post
Kent,

Do you use the Meco when annealing aluminum? Or, do you prefer a larger torch with a heating tip?

What about body leading?

Thanks
Yes, I anneal my aluminum with a 2 or a 3 on the Meco. For larger flames I may go to a 7, and then to my big air-propane weed burner.

I use a 3 or 4 tip when doing autobody lead work, and set a big soft flame.
Sometimes if I am doing a large area I will use a 6 tip set small and soft.
__________________
Kent

http://www.tinmantech.com

"All it takes is a little practical experience to blow the he!! out of a perfectly good theory." --- Lloyd Rosenquist, charter member AWS, 1919.