We have similar materials constraint difficulties here in South Africa. I use 1050 H14 which is half-hard and forms very well. You can always anneal it further if required and I use Sharpie ink to mark the panel prior to heating, and when it vanishes after heating, I know that the metal's beautifully annealed.