Quote:
Originally Posted by Ken Hosford View Post
After posting the Gorilla comment I got to thinking hmmm the way I for motorcycle fenders I get away with not annealing half hard brass , I form 304 stainless and even titanium . So I stopped by Alro service center and picked up a piece of 6061 T6 .050 sheared it up and formed a fender out of it in non annealed state . I was able to do it But my process does not over work it . The 6061 T6 was no worse than stainless or titanium doable

Yep.


Yas, and .... yabetcha.
__________________
Kent

http://www.tinmantech.com

"All it takes is a little practical experience to blow the he!! out of a perfectly good theory." --- Lloyd Rosenquist, charter member AWS, 1919.